PROPIEDAD
|
MÉTODO DE PRUEBA
|
MARV Español
|
||
Tensión de agarre
|
ASTM D-4632
|
200 lbs
|
250 lbs
|
315 lbs
|
Elongación de agarre
|
ASTM D-4632
|
15%
|
15%
|
15%
|
Estallido de Mullen
|
ASTM-D-3786
|
400 psi
|
450 psi
|
600 psi
|
Resistencia a la punción CBR
|
ASTM D-6241
|
700 lbs
|
750 lbs
|
900 lbs
|
Desgarro trapezoidal
|
ASTM-D-4533
|
75 lbs
|
90 lbs
|
125 lbs
|
Resistencia UV (500 horas)
|
ASTM D-4355
|
70%
|
70%
|
70%
|
Permeabilidad
|
ASTM D-4491
|
0.05 seg -¹
|
0.05 seg -¹
|
0.05 seg -¹
|
AOS
|
ASTM-D-4751
|
0.425 mm
|
0.425 mm
|
0.425 mm
|
Tasa de flujo
|
ASTM D-4491
|
5 galones/min/pie cuadrado
|
4 galones/min/pie cuadrado
|
4 galones/min
|