| Product Classification : Hastelloy Alloy | ||||||||||||
| Material : Hastelloy C-276 | ||||||||||||
| Corresponding Brand Number | ||||||||||||
| New Name for High Temperature | Old Name of High Temperature | New Name for Corrosion Resistance | Corrosion Resistant Old Name | National Brand Number | ||||||||
| NS3304 | 00Cr16Ni60Mo164 | |||||||||||
| JIS | ASTM | UNS, SAE | DIN | DIN | ||||||||
| Hastelloy C276 | N10276 | NiCrofer 5916hMoW | 2.4819 | |||||||||
| Chemical Composition | ||||||||||||
| % | C | Si | Mn | P | S | Ni | Cr | Mo | W | Fe | V | |
| Min | <0.02 | ≤0.08 | ≤1.0 | ≤0.04 | ≤0.03 | Allowance | 14.5 | 15 | 3 | 4 | ≤0.35 | |
| Max | / | / | / | / | / | / | 16.5 | 17 | 4.5 | 7 | ||
| Physical Properties | ||||||||||||
| Density g/cm² | Magnetic Properties | Thermal conductivity/w/(m.k) | Electrical resistivity | Specific heat capacity | Coefficient of linear expansion | |||||||
| 100~1092ºC | C)/(Ω.mm2/m) | ºC)/J/(kg.k)ºC | /(10-6/k) | |||||||||
| 20~649ºC | ||||||||||||
| 8.885 | / | 9.4-28 | 1.3 | 427 | 14.1 | |||||||
| Mechanical Properties : (The mechanical properties were tested at 20 °C) | ||||||||||||
| Heat Treatment Mode | Tensile Strength ob/MPa | Strength of Yield σp0.2/MPa | Rate of Elongation σ5 /% | Brinell Hardness HBS | ||||||||
| Solid Solution Treatment | 690 | 283 | 40 | --- | ||||||||
| Production execution standard : | ||||||||||||
| Standards | Bar of Steel | Forging Piece | Board (Strip) Material | Wire Material | Pipe Material | |||||||
| American Society for Materials and Testing | ASTM B574 | ASTM B564 | ASTM B575 |
ASTM B622
ASTM B619 ASTM B626 |
||||||||
| American Technical Code for Aerospace Materials | ||||||||||||
| American Technical Code for Aerospace Materials | ASME SB574 | ASME SB564 | ASME SB575 |
ASTM SB622
ASTM SB619 ASTM SB626 |
||||||||